Difference between revisions of "Aluminum Radiator Repair"
From Pvdwiki
m (→The Solder) |
(→Cleaning the Solder Area) |
||
Line 23: | Line 23: | ||
===Cleaning the Solder Area=== | ===Cleaning the Solder Area=== | ||
+ | Paint stripper, a soft brush, water, and compressed air clean the area fine. | ||
+ | [[Image:Paint-stripper.jpg]] | ||
+ | It foams as it works. | ||
+ | |||
+ | [[Image:Paint-stripper-working.jpg]] | ||
[[Category:Motorcycle]] | [[Category:Motorcycle]] | ||
[[Category:Powerplant]] | [[Category:Powerplant]] |
Revision as of 00:41, 31 July 2007
Tig Welding
The solder did not work for this repair. Nothing seemed to get the solder to stick to the radiator. In the end, I TIG welded the hole. It was tough. I used a 1/16" electrode at 40 amps and 3/32 filler wire. I would have loved a smaller electrode and wire, but this stuff is small as it is.
The Solder
Aluminum solder exists. I could not get it to work.
ALSOLDER 500, PDS-Flow at 482°F.
Stay-Clean Aluminum Flux, PDS- A honey like liquid flux.
Kit Price - $27.37 from Praxair.
The Torch
Mapp gas (C3H4) produces a flame temperature of 5301° F (2927° C)
Propane gas (C3H8) produces a flame temperature of 4325° F (2385°C)
Cleaning the Solder Area
Paint stripper, a soft brush, water, and compressed air clean the area fine.
It foams as it works.